Hydrophilic foil,best price
Hydrophilic foil
1.Coating structure:
///////////////////////////////////////////////// |
\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\ |
|
////////////////////////////////////////////////// |
\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\\ |
----------HYDROPHILICLAYER
--------- ANTI-CORROSIVE LAYER
-----------ALUMINUM FOIL
-----------ANTI-CORROSIVE LAYER
-----------HYDROPHILLC LAYER
2.MECHANICAL PERDORMNCE
ALLOY | TEMPER | THICKNESS MM | TENSILE STRENGHT | ELONGATION ≥ % | ERICHSEN ≥(MM) |
8011 | O | 0.105-0.150 | 95-115N/MM° | 22 | 7.0 |
H22 | 0.09-0.150 | 105-130N/MM° | 20 | 6.5 | |
H24 | 0.09-0.150 | 120-140N/MM° | 16 | 6.0 | |
H26 | 0.095-0.130 | 125-150N/MM° | 12 | 5.5 |
3COATING PROPERTIES
ITEM | SPEC | |
THICKNESS OF COATING | 1.0—2.0 úm | |
ADHESIVE FORCE | HATCHING TEST | SPACKING: 100% |
CUPPING TEST | 5mm DEPTH:100% No DELAMENATION | |
BENDING | 180:NO DELAMENATION | |
INITIAL HYDROPHILICITY | TOUCHING ANGEL | Below 10° |
TOUCHINGANGEL AFTER SKIMMED | Below 20° | |
CONTINOUS HYDROPHILICITY | DIP IN FLOWING WATER | less than 25° |
WEY-DRY CYCLE | less than 30° | |
CORROSION RESISTANCE | CORROSION TESTING | R.NO.≥9.5 |
WETTING TEST | ||
HEAT RESISTANCE | 200°CX5MINS | NO CHANGE |
400°CX5MINS | NO CHANGE |
Hydrophilic foil,best price